MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECASINT 3032 Polyimide, Black, 40% Graphite (PI)
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Graphite Filled

Material Notes: TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance among other things. The TECASINT 2000 series offers these enhanced thermal properties along with lower moisture absorption, a higher degree of toughness, and better machining properties. TECASINT 2011 is unfilled, while TECASINT 2021 contains 15% graphite which offer improved wear resistance and a lower coefficient of friction. TECASINT 2000 series with their superior physical properties, are ideal for application in the aerospace, nuclear, automotive, electrical/electronics, and chemical processing industries.

Main features: High thermal and mechanical capacity, very creep resistant, good radiation-resistance, good sliding properties, broad chemical compatibility, low thermal expansion, no electrical insulation, sensitive to hydrolysis in higher thermal range, flame retardant according to UL94 V-0, low water absorption, high toughness

Applications: Mechanical engineering, automotive industry, materials handling equipment, hot glass technology, aircraft and aerospace industries, cryogenics, precision engineering, textile industry

Preferred Fields: Valve seating, piston rings, chain guides, gripper finger for hot glass, bearing discs, washers, bushings

Information Provided by Ensinger Sintimid

Key Words: PI CS 40
Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³DIN 53 479
Water Absorption  0.54 %
@Temperature 23.0 °C
0.54 %
@Temperature 73.4 °F
24 hours in water; EN ISO 62
 3.15 %
@Temperature 80.0 °C
3.15 %
@Temperature 176 °F
24 hours in water; EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80
@Temperature 23.0 °C
80
@Temperature 73.4 °F
DIN 53 505
Tensile Strength 41.6 MPa
@Temperature 23.0 °C
6030 psi
@Temperature 73.4 °F
EN ISO 527
Elongation at Break 2.2 %
@Temperature 23.0 °C
2.2 %
@Temperature 73.4 °F
EN ISO 527
Tensile Modulus 3.524 GPa
@Temperature 23.0 °C
511.1 ksi
@Temperature 73.4 °F
EN ISO 527
Flexural Strength 68.0 MPa
@Temperature 23.0 °C
9860 psi
@Temperature 73.4 °F
EN ISO 178
Flexural Modulus 3.865 GPa
@Temperature 23.0 °C
560.6 ksi
@Temperature 73.4 °F
EN ISO 178
Flexural Strain at Yield 2.2 %
@Temperature 23.0 °C
2.2 %
@Temperature 73.4 °F
EN ISO 178
Compressive Yield Strength 87.0 MPa
@Strain 10 %,
Temperature 23.0 °C
12600 psi
@Strain 10 %,
Temperature 73.4 °F
EN ISO 604
Compressive Strength 133 MPa
@Temperature 23.0 °C
19300 psi
@Temperature 73.4 °F
EN ISO 604
Compressive Modulus 1.044 GPa
@Temperature 23.0 °C
151.4 ksi
@Temperature 73.4 °F
EN ISO 604
Charpy Impact Unnotched 1.07 J/cm²
@Temperature 23.0 °C
5.09 ft-lb/in²
@Temperature 73.4 °F
EN ISO 179
Charpy Impact, Notched 0.300 J/cm²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
EN ISO 179
Compression Set 29 %
@Temperature 23.0 °C
29 %
@Temperature 73.4 °F
Compression at Break; EN ISO 604
 
Thermal PropertiesMetricEnglishComments
CTE, linear  31.0 µm/m-°C
@Temperature 50.0 - 200 °C
17.2 µin/in-°F
@Temperature 122 - 392 °F
DIN 53 752
 40.0 µm/m-°C
@Temperature 200 - 300 °C
22.2 µin/in-°F
@Temperature 392 - 572 °F
DIN 53 752

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger TECASINT 5051 Polyimide, 30% Glass Fiber Filled (PI)
Hippe PI
Ensinger TECASINT 1041 Polyimide, 30% MoS2 Filled (PI)
Ensinger TECASINT 4011 Polyimide, Yellow (PI)
Ensinger TECASINT 4041 Polyimide, Glossy Black, Molybdenum Sulfide (PI)

PENSIN078 / 121081

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.