System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Covestro Bayflex® 180 Polyurethane Elastomeric RIM, 20% Mica Filled, MDI-based 2-Component Liquid System
(discontinued **)
Categories:
Polymer
;
Thermoset
;
Filled/Reinforced Thermoset
;
Polyurethane, TS
;
Thermoset Polyurethane, Elastomer, Glass Filled
;
Rubber or Thermoset Elastomer (TSE)
Material Notes:
0.150 in. thickness. RIM = Reaction Injection Molding
Information provided by Bayer Corporation, Polyurethanes Division
As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.25
g/cc
0.0452
lb/in³
ASTM D792
Water Absorption at Saturation
0.20 %
0.20 %
240 hours; Bayer Test
Linear Mold Shrinkage
0.0055
cm/cm
0.0055
in/in
Bayer Test
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
35.0
MPa
5080
psi
ASTM D638/D412
Elongation at Break
22 %
22 %
ASTM D638/D412
Flexural Modulus
2.07
GPa
300
ksi
ASTM D790
Izod Impact, Notched
1.10
J/cm
2.06
ft-lb/in
ASTM D256
Tear Strength
140
kN/m
799
pli
Die C; ASTM D624
Thermal Properties
Metric
English
Comments
CTE, linear
135
µm/m-°C
@Temperature 20.0 °C
75.0
µin/in-°F
@Temperature 68.0 °F
ASTM D696
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Covestro Baydur® 110 FR Polyurethane
Covestro Baydur® 60 Polyurethane
Covestro Bayflex® 110-50 CM Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Covestro Baydur® GS PUR Polyurethane
Covestro Bayflex® 190 Polyurethane Elastomeric RIM, 20% Mica Filled, MDI-based 2-Component Liquid System
PB2B79 / 26621
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.