Ovation Polymers UTTAP™ SF 50030 GF Polyether Sulfone, 30% Glass Fiber
Categories:
Polymer
;
Thermoplastic
;
Polyethersulfone (PES)
;
Polyethersulfone (PES), 30%Glass Fiber Filled
Material Notes:
Excellent chemical and electrical resistance, high stiffness, modulus and HDT
All properties after 48hrs conditioning at 23°C/50% RH
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.62
g/cc
1.62
g/cc
ASTM D792
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
169
MPa
24500
psi
50 mm/min; ASTM D638
Elongation at Break
3.5 %
3.5 %
50 mm/min; ASTM D638
Tensile Modulus
6.60
GPa
957
ksi
50 mm/min; ASTM D638
Flexural Strength
221
MPa
32100
psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus
11.3
GPa
1640
ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched
0.801
J/cm
@Temperature 23.0 °C
1.50
ft-lb/in
@Temperature 73.4 °F
ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
>=
210
°C
@Thickness 3.20 mm
>=
410
°F
@Thickness 0.126 in
Unannealed; ASTM D648
Glass Transition Temp, Tg
225
°C
437
°F
ASTM D3482
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Ovation Polymers UTTAP SF 50030GF Polyethersulfone, 30% Glass Reinforced
Ovation Polymers Nima™ NH PC143P Polycarbonate
Ovation Polymers Nemcon™ H PO DP 117/X2 Polyolefin, Thermally conductive
Ovation Polymers OpteSTAT™ NC PES 6010 Polyether Sulfone based Carbon Nanotube Compound
Ovation Polymers OpteSTAT™ NC PPS 7010 Polyphenylenesulfide based Carbon Nanotube Compound
POVAT157 / 79136
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.