MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Rogers Corporation Bisco® A2 Sound Barrier Engineered Solid Silicone Mass Layer, Sound Barrier
Categories: Polymer; Thermoset; Silicone; Silicone Foam

Material Notes: BISCO® A2 Sound Barrier is a solid silicone rubber engineered to meet demanding requirements for flammability, smoke density and toxicity. A2 is used to block the transmission of sound and demonstrates excellent performance in low frequency noise reduction. Innovative filler technology is used to create superior flame resistance meeting the radiant panel flammability test FAR25.856(a).
A2 is light gray in color.

Applications:

  • Aircraft acoustic insulation
  • Noise reduction liner for interior panels
  • Aircraft flooring noise barrier
  • Rail Interior noise blocker

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.64 g/cc0.0592 lb/in³ISO 2781
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6262ISO 868
Tensile Strength 2.80 MPa406 psiISO 37 Type 2
Elongation at Break 220 %220 %ISO 37 Type 2
Tear Strength 10.2 kN/m58.2 pliISO 34 Method C
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 °C356 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Descriptive Properties
Flammability TestPassJAR/FAR, Part 25, App. F Part 1, Para (a) (1) (ii) and Part III [change 15/Amdt. 25-60] and Part VI
Polymer TypeVMQISO 1629
Smoke Density (min)Passes smoke gas components test AITM3.0005JAR/FAR 25, App. F, Part V & AITM 2.0007

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATG s.r.l. AU-EU Polyurethane Rubber
DuPont™ Nomex® 410 Paper, 2 mil Nominal Thickness
BASF Ultraform® N2650 Z4 POM + PUR
Multibase Multi-Flex® TPE A 8699 BLK
Lanxess Urepan® 640 G Polyurethane Rubber

PROGA906 / 138346

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.