MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

INEOS Styrolution Terblend® N NG-02 EF 8% Glass Filled ABS+PA (Conditioned)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced; Nylon (Polyamide PA)

Material Notes: Terblend® N NG-02 EF is an 8% glass fiber reinforced UV-stabilized ABS/PA blend with enhanced dimensional stability, rigidity and high flowability. High dimensional stability, Excellent flow for high surface quality appearance, Enhanced softening temperature, Enhanced rigidity, UV-stabilized.

Applications: Automotive parts, Motorcycle fairings, Truck cabin parts

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.3 %1.3 %23°C/50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inISO 2577
Melt Flow 44.8 g/10 min
@Load 10.0 kg,
Temperature 240 °C
44.8 g/10 min
@Load 22.0 lb,
Temperature 464 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 62.0 MPa
@Load 36.5 kg,
Time 30.0 sec
8990 psi
@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Tensile Strength, Yield 40.0 MPa5800 psiISO 527-1/-2
Elongation at Break 12 %12 %Nominal, 50 mm/min; ISO 527-1/-2
Elongation at Yield 4.0 %4.0 %ISO 527-1/-2
Tensile Modulus 2.40 GPa348 ksiISO 527-1/-2
Izod Impact, Notched (ISO)  5.00 kJ/m²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 25.0 kJ/m²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched  3.50 J/cm²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmIEC 60093
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.090
@Frequency 1e+6 Hz
0.090
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 118 °C244 °FVST/B/50; ISO 306
 200 °C392 °FVST/A/50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 270 °C464 - 518 °FInjection Molding
Mold Temperature 40.0 - 80.0 °C104 - 176 °FInjection Molding
 
Descriptive Properties
ColorNatural
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Daicel CEVIAN® A2606 30% GF PA/ABS Alloy, DAM
Daicel CEVIAN® A2606 30% GF PA/ABS Alloy, Conditioned
Aclo Accucomp Polypropylene HPO306L Homopolymer
INEOS Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Conditioned)
INEOS Styrolution Terblend® N NM-13 ABS+PA (Conditioned)

PBASG0603 / 132236

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.