MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Syensqo (Solvay Specialty Polymers) Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), Mineral Filled

Material Notes: AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage. Excellent dimensional stability and low moisture absorption are also characteristics of this resin.

AMODEL A-1340 HS resin can be easily processed using conventional equipment and methods.

Information provided by Solvay Advanced Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.48 g/cc1.48 g/ccISO 1183A
 1.54 g/cc1.54 g/ccASTM D792
Moisture Absorption at Equilibrium 0.16 %0.16 %24 hours; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 125125ASTM D785
Tensile Strength, Yield 151 MPa21900 psiISO 527
 174 MPa25200 psiASTM D638
 46.0 MPa
@Temperature 175 °C
6670 psi
@Temperature 347 °F
ISO 527
 49.0 MPa
@Temperature 150 °C
7110 psi
@Temperature 302 °F
ISO 527
 97.0 MPa
@Temperature 100 °C
14100 psi
@Temperature 212 °F
ISO 527
Elongation at Break 1.8 %1.8 %ISO 527
 2.3 %
@Temperature 100 °C
2.3 %
@Temperature 212 °F
ISO 527
 7.0 %
@Temperature 175 °C
7.0 %
@Temperature 347 °F
ISO 527
 7.4 %
@Temperature 150 °C
7.4 %
@Temperature 302 °F
ISO 527
Elongation at Yield 2.2 %2.2 %ASTM D638
Tensile Modulus 11.0 GPa1600 ksiASTM D638
 11.6 GPa1680 ksiISO 527
 2.70 GPa
@Temperature 175 °C
392 ksi
@Temperature 347 °F
ISO 527
 3.10 GPa
@Temperature 150 °C
450 ksi
@Temperature 302 °F
ISO 527
 8.00 GPa
@Temperature 100 °C
1160 ksi
@Temperature 212 °F
ISO 527
Flexural Strength 234 MPa33900 psiISO 178
 263 MPa38100 psiASTM D790
 55.0 MPa
@Temperature 175 °C
7980 psi
@Temperature 347 °F
ISO 178
 63.0 MPa
@Temperature 150 °C
9140 psi
@Temperature 302 °F
ISO 178
 155 MPa
@Temperature 100 °C
22500 psi
@Temperature 212 °F
ISO 178
Flexural Modulus 9.10 GPa1320 ksiISO 178
 10.6 GPa1540 ksiASTM D790
 2.30 GPa
@Temperature 175 °C
334 ksi
@Temperature 347 °F
ISO 178
 2.50 GPa
@Temperature 150 °C
363 ksi
@Temperature 302 °F
ISO 178
 6.80 GPa
@Temperature 100 °C
986 ksi
@Temperature 212 °F
ISO 178
Poissons Ratio 0.380.38
Shear Modulus 3.99 - 4.20 GPa579 - 609 ksiCalculated
Shear Strength 91.0 MPa13200 psiASTM D732
Izod Impact, Notched 0.450 J/cm0.843 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) 31.0 kJ/m²14.8 ft-lb/in²ISO 180/1U
Charpy Impact Unnotched 4.50 J/cm²21.4 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.330 J/cm²1.57 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+15 ohm-cm2.00e+15 ohm-cmASTM D257
 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant  4.3
@Frequency 1e+6 Hz
4.3
@Frequency 1e+6 Hz
ASTM D150
 4.5
@Frequency 100 Hz
4.5
@Frequency 100 Hz
ASTM D150
Dissipation Factor  0.0050
@Frequency 100 Hz
0.0050
@Frequency 100 Hz
ASTM D150
 0.017
@Frequency 1e+6 Hz
0.017
@Frequency 1e+6 Hz
ASTM D150
High Voltage Arc Resistance to Ignition (HVAR) 150 sec150 secASTM D495
Comparative Tracking Index 550 V550 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  19.0 µm/m-°C
@Temperature 160 - 250 °C
10.6 µin/in-°F
@Temperature 320 - 482 °F
 29.0 µm/m-°C
@Temperature 0.000 - 100 °C
16.1 µin/in-°F
@Temperature 32.0 - 212 °F
CTE, linear, Transverse to Flow  46.0 µm/m-°C
@Temperature 0.000 - 100 °C
25.6 µin/in-°F
@Temperature 32.0 - 212 °F
 92.0 µm/m-°C
@Temperature 160 - 250 °C
51.1 µin/in-°F
@Temperature 320 - 482 °F
Melting Point 313 °C595 °FISO 11357-3
 313 °C595 °FASTM D3418
Maximum Service Temperature, Air 130 °C266 °F20000 hours, Continuous; ASTM D3045
 150 °C302 °F5000 hours, Continuous; ASTM D3045
Deflection Temperature at 0.46 MPa (66 psi) 290 °C554 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 262 °C504 °FISO 75Af
 275 °C527 °FASTM D648
Flammability, UL94 HBHB

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOLVT62 / 21358

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.