MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Lucas-Milhaupt Silvaloy® A20 Brazing Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Silvaloy A20 can be used in a wide variety of applications but is infrequently used because of its relatively high melting point. It is an excellent choice when simultaneously brazing and heat treating carbon steel because of the close temperature match. It is also widely used on yellow brass assemblies because of the close color match. Generally, the strength of Silvaloy A20 will surpass the strengths of the base metals.

Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 712.8 - 816 °C1315 - 1500 °F
Solidus 712.8 °C1315 °F
Liquidus 816 °C1500 °F
Maximum Service Temperature, Air 149 °C300 °Fcontinuous
 260 °C500 °Fintermittent
 
Processing PropertiesMetricEnglishComments
Processing Temperature 816 - 871 °C1500 - 1600 °FBrazing Temperature
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 44 - 46 %44 - 46 %
Silver, Ag 19 - 21 %19 - 21 %
Zinc, Zn 33 - 37 %33 - 37 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver
Overview of materials for Silver Alloy
Lucas-Milhaupt Cerametil 616 Active Metal Brazing
Cadi 50WS Tungsten Silver
ATI Allvac® Nickelvac® HC-276 Nickel Superalloy, Heat Treatment: 1121°C (2050°F) Anneal

NBRW018 / 79794

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.