MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

3M Dyneon™ TFM™ 4215 Modified PTFE, 25% Electrocarbon Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Conductive Carbon Filled

Material Notes: Applications include bearings, seals/gaskets, packings, piston rings.

Data provided by Dyneon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.11 g/cc0.0762 lb/in³Sintered moldings; ASTM D4894/D4895
Apparent Bulk Density 0.750 g/cc0.0271 lb/in³DIN 53 466
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6666ASTM D2240
Tensile Strength, Ultimate 13.0 MPa
@Thickness 2.00 mm
1890 psi
@Thickness 0.0787 in
ASTM D4894
Elongation at Break 70 %
@Thickness 2.00 mm
70 %
@Thickness 0.0787 in
ASTM D4894
 
Thermal PropertiesMetricEnglishComments
Shrinkage 3.3 %
@Thickness 80.0 mm
3.3 %
@Thickness 3.15 in
sheet; ASTM D4894

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Dyneon™ TFM™ 4212 Modified PTFE, 10% Electrocarbon Filled
3M Dyneon™ TFM™ 1700 Granular, PTFE
3M Dyneon™ TFM™ 1600 PTFE
3M Dyneon™ TFM™ 1700 PTFE
3M Dyneon™ TFM™ 1700 Modified PTFE Powder

PDYM86 / 34689

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.