System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Plaskolite Duraplex® SG-10 Sign Grade Acrylic Sheet, Impact Modified
Categories:
Polymer
;
Thermoplastic
;
Acrylic (PMMA)
;
Acrylic, Optical Sheet
Material Notes:
Available in unlimited lengths - no seams in finished products.
Data provided by the manufacturer, Plaskolite, Inc.
Key Words:
PMMA; Polymethyl Methacrylate
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.15
g/cc
0.0415
lb/in³
ASTM D792
Water Absorption
0.30 %
0.30 %
ASTM D570
Linear Mold Shrinkage
0.0030
-
0.0060
cm/cm
0.0030
-
0.0060
in/in
ASTM D955
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
46
46
Method A; ASTM D785
Tensile Strength, Yield
39.0
MPa
5660
psi
ASTM D638
Tensile Modulus
1.70
GPa
247
ksi
ASTM D638
Flexural Yield Strength
57.0
MPa
8270
psi
ASTM D790
Izod Impact, Notched
1.10
J/cm
2.06
ft-lb/in
ASTM D256
0.500
J/cm
@Temperature -18.0 °C
0.937
ft-lb/in
@Temperature -0.400 °F
ASTM D256
Gardner Impact
5.30
J
3.91
ft-lb
reported as J/cm; ASTM D3029-GB, unpainted
Thermal Properties
Metric
English
Comments
CTE, linear
90.0
µm/m-°C
@Temperature -18.0 - 38.0 °C
50.0
µin/in-°F
@Temperature -0.400 - 100 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)
82.0
°C
180
°F
annealed; ASTM D648
Optical Properties
Metric
English
Comments
Haze
3.0 %
3.0 %
ASTM D1003
Transmission, Visible
90 %
90 %
ASTM D1003
Processing Properties
Metric
English
Comments
Processing Temperature
154
°C
309
°F
Optimal Thermoforming temperature for sheet 0.25-1.0 cm (0.10-0.39 in)
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Plaskolite Duraplex® 100% I Impact Modified Acrylic Sheet
Overview of materials for Acrylic, General Purpose, Molded
Plaskolite Duraplex® SG-05 Sign Grade Acrylic Sheet, Impact Modified
Overview of materials for Acrylic, Optical Sheet
Overview of materials for Acrylic, Optical Grade, Molded
PPLASD / 56286
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.