MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Sandvik Sanicro 36Mo logging cable Precision Wire
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: Sandvik Sanicro 36Mo is a nitrogen enhanced high alloyed austenitic stainless alloy for service in extreme conditions in the oil and gas industry. It is characterized by:
  • Excellent corrosion resistance in chloride and acidizing environments owing to its high PRE*) value of minimum 50.
  • Extreme resistance to sour conditions
  • Very high tensile strength
  • Information provided by Sandvik

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 8.00 g/cc0.289 lb/in³
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength, Ultimate >= 2070 MPa>= 300000 psi
    Tensile Strength, Yield >= 1758 MPa
    @Strain 0.2 %
    >= 255000 psi
    @Strain 0.2 %
    Modulus of Elasticity 190 GPa27600 ksi
     
    Electrical PropertiesMetricEnglishComments
    Electrical Resistivity 0.000105 ohm-cm0.000105 ohm-cm
    Magnetic Permeability <= 1.003
    @Temperature 20.0 °C
    <= 1.003
    @Temperature 68.0 °F
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear  14.5 µm/m-°C
    @Temperature 30.0 - 100 °C
    8.06 µin/in-°F
    @Temperature 86.0 - 212 °F
     15.5 µm/m-°C
    @Temperature 30.0 - 300 °C
    8.61 µin/in-°F
    @Temperature 86.0 - 572 °F
    Specific Heat Capacity  0.470 J/g-°C
    @Temperature 20.0 - 100 °C
    0.112 BTU/lb-°F
    @Temperature 68.0 - 212 °F
     0.500 J/g-°C
    @Temperature 100 - 200 °C
    0.120 BTU/lb-°F
    @Temperature 212 - 392 °F
     0.510 J/g-°C
    @Temperature 200 - 300 °C
    0.122 BTU/lb-°F
    @Temperature 392 - 572 °F
     
    Component Elements PropertiesMetricEnglishComments
    Carbon, C <= 0.020 %<= 0.020 %
    Chromium, Cr 27 %27 %
    Iron, Fe 27.7 %27.7 %As Balance
    Manganese, Mn 5.0 %5.0 %
    Molybdenum, Mo 5.4 %5.4 %
    Nickel, Ni 34 %34 %
    Nitrogen, N 0.40 %0.40 %
    Phosphorus, P <= 0.020 %<= 0.020 %
    Silicon, Si <= 0.50 %<= 0.50 %
    Sulfur, S <= 0.010 %<= 0.010 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 204°C Temper
    AIM 47 Fusible Bismuth Alloy
    AIM 35.7Sn/35.7Pb/28.6Bi Solder for Photonic Packaging
    ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 204°C Temper
    ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 288°C Temper

    NSANDV219 / 19113

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.