Radici Radilon® A 50HSKB 870 M BR Polyamide 66
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Extruded
;
Nylon 66, Heat Stabilized
Material Notes:
PA66 high viscosity extrusion grade. Internally lubricated. Heat stabilized. DPPD free. Natural brown color. Suitable for extrusion of pipes, intended for use in contact with oil and grease.
Information provided by Radici Group.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.12
g/cc
0.0405
lb/in³
DAM; ISO 1183
Water Absorption
8.9 %
@Thickness 2.00 mm,
Temperature 23.0 °C
8.9 %
@Thickness 0.0787 in,
Temperature 73.4 °F
Immersion; ISO 62
Moisture Absorption
2.10 %
@Thickness 2.00 mm,
Temperature 23.0 °C
2.10 %
@Thickness 0.0787 in,
Temperature 73.4 °F
50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.011
cm/cm
0.011
in/in
Conditioned; ISO 294-4
0.011
cm/cm
0.011
in/in
DAM; ISO 294-4
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
80.0
MPa
11600
psi
50mm/min. DAM; ISO 527-2/1A
Elongation at Break
55 %
55 %
50mm / min. DAM. Nominal.; ISO 527-2/1A
Elongation at Yield
4.5 %
4.5 %
DAM; ISO 527-2/1A
Tensile Modulus
3.10
GPa
450
ksi
1mm / min. DAM; ISO 527-2/1A
Flexural Strength
115
MPa
16700
psi
2mm / min. DAM; ISO 178
Flexural Modulus
3.00
GPa
435
ksi
2mm / min. DAM; ISO 178
Charpy Impact, Notched
0.550
J/cm²
@Temperature -30.0 °C
2.62
ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+11
ohm-cm
1.00e+11
ohm-cm
Conditioned. 500V; IEC 60093
1.00e+13
ohm-cm
1.00e+13
ohm-cm
DAM; 500V.; IEC 60093
Surface Resistance
1.00e+10
ohm
1.00e+10
ohm
Conditioned. 500V; IEC 60093
1.00e+12
ohm
1.00e+12
ohm
DAM; 500V.; IEC 60093
Thermal Properties
Metric
English
Comments
Melting Point
260
°C
500
°F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi)
80.0
°C
176
°F
ISO 75/2Af
Vicat Softening Point
240
°C
@Load 5.10 kg
464
°F
@Load 11.2 lb
50°C/h; ISO 306
Flame Spread
0.000
mm/min
@Thickness 3.00 mm
0.000
in/min
@Thickness 0.118 in
Automotive Interior; ISO 3795
Processing Properties
Metric
English
Comments
Processing Temperature
270
-
290
°C
518
-
554
°F
Extrusion Temperature
Melt Temperature
280
-
300
°C
536
-
572
°F
Injection Molding
Mold Temperature
70.0
-
90.0
°C
158
-
194
°F
Descriptive Properties
Injection Molding Injection Speed
Medium
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PRADI6912 / 293417
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.