MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

EMS-Grivory Grilamid® LV-15H nat PA12-GF15
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 20% Glass Fiber Filled

Material Notes: Product description: Grilamid LV-15H is a 15% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile:
  • very low water absorption
  • good dimensional stability
  • very high elongation
  • good chemical resistance
  • good UV stability
  • high impact strength
Grilamid LV-15H is suitable for the manufacturing of technical parts in the application fields of:
  • Electrical and electronic components
  • Automotive
  • Safety parts
  • Mechanical engineering
  • Domestic appliances
  • Analytical and mecical devices
  • Sports & leisure goods

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³Dry; ISO 1183
Water Absorption 1.3 %1.3 %Sim. to ISO 62
Moisture Absorption 0.800 %0.800 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 74
@Time 15.0 sec
74
@Time 0.00417 hour
Conditioned; ISO 868
Tensile Strength at Break 70.0 MPa10200 psiConditioned; ISO 527-1/-2
 80.0 MPa11600 psiDry; ISO 527-1/-2
Elongation at Break 8.0 %8.0 %Dry; ISO 527-1/-2
 10 %10 %Conditioned; ISO 527-1/-2
Tensile Modulus 3.00 GPa435 ksiConditioned; ISO 527-1/-2
 3.50 GPa508 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  7.50 J/cm²
@Temperature 23.0 °C
35.7 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 7.50 J/cm²
@Temperature -30.0 °C
35.7 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 35.0 kV/mm889 kV/inConditioned; IEC 60243-1
Comparative Tracking Index 600 V600 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C22.2 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C44.4 µin/in-°FISO 11359-1/-2
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C194 - 248 °FLong Term; ISO 2578
 150 °C302 °FShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 150 °C302 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 80.0 °C176 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Compressed air systems
 Cooling and climate control
 Fuel systems
 Hydraulic systems
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical appliances
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Medical devices
 Power transmission
 Sanitary, water and gas supply
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Product AttributesHydrolysis resistant
Special CharacteristicsHigh impact or impact modified
 Improved heat resistance
 Improved UV resistance (outdoor use)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
301 Stainless Steel
Multibase TPSiV® 4000-70A Thermoplastic Silicone Vulcanizate
Alclad Aluminum 6061-T6, T651
Alliance N-42H Neodymium Iron Boron Magnetic Material
410 Stainless Steel

PGRH071 / 156780

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.