MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

SABIC ULTEM™ DIELECTRIC FILM for small to medium size capacitors UTF120
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: ULTEM™ UTF120 dielectric PEI film offers solutions for small to medium size, professional-grade capacitors, up to 10 microfarads capacitance, addressing challenging industry requirements. The film exhibits stable properties through a range of temperatures (-40 °C to +150 °C) and frequency, including stable capacitance, good insulation resistance, stable dielectric constant (Dk) and low dissipation factor (Df). ULTEM UTF120 film has been validated by customers with both film-foil and metalized electrodes, including flat aluminum, heavy edge/light body and fused/patterned electrode designs. ULTEM UTF120 film offers excellent handling through metallization, winding and capacitor squashing / flattening. Additionally, capacitors using ULTEM UTF120 film are also capable of passing industry-standard 260 °C reflow soldering processes. ULTEM UTF120 dielectric film is available in 4, 5, 7 & 10 micron gauges sold in 620mm x 5000m size rolls.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ASTM D792
Moisture Absorption at Equilibrium 0.23 %0.23 %23°C/50% RH; ASTM D570
Water Absorption at Saturation 1.16 %1.16 %ASTM D570

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80014 / 287961

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.