MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Tin Bronze, UNS C90500, Copper Casting Alloy, M01 Temper, As Sand Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Sand Cast

Casting Characteristics: High – Effect of Section Size; Medium – Casting Yield, Gassing, Fluidity, Shrinkage in Solidification; Low - Drossing

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability - Brazing; Fair Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding

Typical uses: Clamps; Heavy Construction Equipment; Connectors; Nuts; Bearings; Bushings; Expansion Bearings; Finishing Dies for Wood Pulp Industry; Gear Blanks; Gears; Piston Rings; Pump Bodies; Pump Impellers; Seal Rings; Valve Bodies; Valves; Worm Gears; Steam Fittings; Water Conditioners

Applicable Specifications: As Centrifugal Cast – Castings SAE J462; Castings SAE J461, Castings ASTM B271/B271M, Castings AMS 4845; As Continuous Cast – Castings ASTM B505/B505M, Castings SAE J462, Castings SAE J461; As Sand Cast – Castings SAE J461, Castings AMS 4845, Castings SAE J462, Castings ASTM B584, Castings ASTM B22/B22M, Castings ASTM B763/B763M; Ingot - ASTM B30; Precision Cast – Castings MILITARY MIL-C-11866

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.72 g/cc0.315 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 7575
Tensile Strength >= 276 MPa>= 40000 psifor Standard
 310 MPa45000 psiTypical
Tensile Strength, Yield >= 124 MPa>= 18000 psifor Standard, 0.5% Ext
 152 MPa22000 psiTypical, 0.5% Ext
Elongation at Break >= 20 %>= 20 %for Standard
 25 %25 %Typical
Reduction of Area 40 %40 %
Tensile Modulus 103 GPa15000 ksi
Compressive Strength 276 MPa40000 psi0.01 in. set/in.
Fatigue Strength 89.6 MPa
@# of Cycles 1.00e+8
13000 psi
@# of Cycles 1.00e+8
Machinability 30 %30 %
Izod Impact 13.6 J10.0 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000156 ohm-cm0.0000156 ohm-cm11% IACS
Magnetic Permeability 1.01.0
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.8 µm/m-°C
@Temperature 20.0 - 300 °C
11.0 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 6.23 W/m-K43.2 BTU-in/hr-ft²-°F
Melting Point 854 - 999 °C1570 - 1830 °F
Solidus 854 °C1570 °F
Liquidus 999 °C1830 °F
Shrinkage 1.56 %1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FStress Relief
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.0050 %<= 0.0050 %
Antimony, Sb <= 0.20 %<= 0.20 %
Copper, Cu 86 - 89 %86 - 89 %
Iron, Fe <= 0.20 %<= 0.20 %
Lead, Pb <= 0.30 %<= 0.30 %
Nickel, Ni <= 1.0 %<= 1.0 %
Phosphorus, P <= 0.050 %<= 0.050 %
Silicon, Si <= 0.0050 %<= 0.0050 %
Sulfur, S <= 0.050 %<= 0.050 %
Tin, Sn 9.0 - 11 %9.0 - 11 %
Zinc, Zn 1.0 - 3.0 %1.0 - 3.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC90500x3 / 293192

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.