MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 2582 HEC FR Polycarbonate/ABS Alloy (PC/ABS) Nickel-Coated Carbon Fiber - EMI/RFI Shielding - Electrically Conductive - Flame Retardant - UL94 V-0
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, NCG Fiber Filled; Polycarbonate (PC)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.37 g/cc1.37 g/ccASTM D 792
Additive Loading 15 %15 %Primary Additive
Linear Mold Shrinkage 0.00050 - 0.0025 cm/cm
@Thickness 3.20 mm
0.00050 - 0.0025 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 113 MPa16400 psiASTM D 638
Elongation at Break 1.0 - 2.0 %1.0 - 2.0 %ASTM D 638
Tensile Modulus 8.27 GPa1200 ksiASTM D 638
Flexural Strength 152 MPa22000 psiASTM D 790
Flexural Modulus 8.27 GPa1200 ksiASTM D 790
Izod Impact, Notched 0.374 J/cm
@Thickness 3.20 mm
0.700 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 3.10 J/cm
@Thickness 3.20 mm
5.80 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 10 ohm-cm<= 10 ohm-cmASTM D 257
Surface Resistance <= 1000 ohm<= 1000 ohmESD STM11.11
Surface Resistivity per Square <= 10000 ohm<= 10000 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 sec<= 0.50 secFTMS101C; 4046.1
Shielding Effectiveness  73 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
73 dB
@Thickness 0.0787 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 80 dB
@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
80 dB
@Thickness 0.118 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 81 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
81 dB
@Thickness 0.0787 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 87 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
87 dB
@Thickness 0.0787 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 88 dB
@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
88 dB
@Thickness 0.118 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 95 dB
@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
95 dB
@Thickness 0.118 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 95 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
95 dB
@Thickness 0.0787 in,
Frequency 1e+9 Hz
ASTM D 4935
 100 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
100 dB
@Thickness 0.0787 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 100 dB
@Thickness 3.00 mm,
Frequency 1e+9 Hz
100 dB
@Thickness 0.118 in,
Frequency 1e+9 Hz
ASTM D 4935
 101 dB
@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
101 dB
@Thickness 0.118 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 102 dB
@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
102 dB
@Thickness 0.118 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 105 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
105 dB
@Thickness 0.0787 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 243 - 274 °C470 - 525 °F
Mold Temperature 51.7 - 93.3 °C125 - 200 °F
Drying Temperature 93.3 °C
@Time 14400 sec
200 °F
@Time 4.00 hour
Moisture Content 0.020 %0.020 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo PULSE™ 2000 EZ PC/ABS Engineering Resin
Mitsubishi Iupilon® EHR 3400 Polycarbonate
Covestro Makrolon® GF9002 Polycarbonate, 10% Glass Filled

PQZWA2518 / 91196

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.