MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Parker Chomerics Tecknit Teckshield®-F 100 OPI 0.0022" Diameter Wire, High Performance EMC Window
Categories: Ceramic; Glass; Optical; Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Sheet

Material Notes: Description: TECKSHIELD-F high-performance fully laminated flat windows are specially designed to provide optimum optical transmission and EMI shielding in severe interference environments. TECKSHIELD-F windows have proven to be effective in TEMPEST qualified Visual Display Units, as well as in printers and enclosures requiring large viewing apertures. A special low-resistance mesh is laminated between two layers of glass or acrylic. The edge termination between the window mesh and the enclosure is designed to provide uniform mesh-to-enclosure continuity around the entire perimeter of the shielding aperture.

Application Information: TECKSHIELD-F high-performance flat windows are designed for enclosures requiring superior shielding against EMI radiation or susceptibility. They provide maximum EMI protection and high optical clarity for teleprinters, digital, graphic, and other flat displays. TECKSHIELD-F windows can also be economically matched to most visual display units to minimize image distortion and to maximize shielding effectiveness.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesMetricEnglishComments
Shielding Effectiveness  40 dB
@Frequency 1e+10 Hz
40 dB
@Frequency 1e+10 Hz
Plane Wave
 55 dB
@Frequency 100000 Hz
55 dB
@Frequency 100000 Hz
H-Field
 60 dB
@Frequency 1e+9 Hz
60 dB
@Frequency 1e+9 Hz
Plane Wave
 120 dB
@Frequency 1e+7 Hz
120 dB
@Frequency 1e+7 Hz
E-Field
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 60.0 °C140 °FAcrylic
 80.0 °C176 °FGlass
Minimum Service Temperature, Air -55.0 °C-67.0 °FGlass
 -55.0 °C-67.0 °FAcrylic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics Tecknit Teckshield®-F 100 OPI 0.002" Diameter Wire, Allycarbonate EMI Shielding Window
Henkel Electrodag® 440 AS EMC Coating
Corning Gorilla® Glass 5 Display Glass
Chi Mei Acryrex® CM-211 PMMA
Corning Gorilla® Glass SR+ Touch Screen Glass

PCHOME393 / 131103

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.