  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Techmer ES Electrafil® DB-1200/SS/7 ABS, 7% Stainless Steel Fiber Reinforced (dry blend)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled

Material Notes: Superior cost-performance when compared with other electrically conductive resins is a hallmark of Electrafil stainless steel fiber reinforced ABS. Electrafil compounds can be formulated to meet UL 94 V-0 requirements, and they provide good dimensional stability, exceptional colorability and appearance. Specify Electrafil stainless steel fiber reinforced ABS for protection from electrostatic discharge (ESD) in applications such as paper path parts for business machines, and for electromagnetic/radio frequency interference (EMI/RFI) shielding in business machine covers and hand-held electronic devices.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
@Thickness 3.17 mm
0.0040 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 40.0 MPa5800 psiASTM D638
Elongation at Break 4.5 %4.5 %ASTM D638
Flexural Yield Strength 78.6 MPa11400 psiASTM D790
Flexural Modulus 2.96 GPa430 ksiASTM D790
Izod Impact, Notched 0.641 J/cm
@Thickness 3.17 mm
1.20 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.100 - 1.00 ohm-cm0.100 - 1.00 ohm-cmASTM C611
Surface Resistance 1.0 - 10 ohm1.0 - 10 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C190 °FASTM D648
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Vestamid® L-R1-MHI Antistatic, Black, Electrically Conductive Nylon 12
Precision Polymer Engineering S70L Conductive Silicone Rubber
Premix Thermoplastics PRESEAL® TPE 6071
Armacell Monarch® F-03091 (Black) Pure EPDM Foam
Armacell Ensolite™ EF0 EPDM crushed foam

PTLCOM003 / 70567

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.