Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.15 g/cc | 1.15 g/cc |
Additive Loading | 10 % | 10 % |
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm | 0.0040 - 0.0060 in/in @Thickness 0.126 in |
|
Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength at Break | 40.0 MPa | 5800 psi |
Elongation at Break | 3.0 - 7.0 % | 3.0 - 7.0 % |
Tensile Modulus | 2.76 GPa | 400 ksi |
Flexural Strength | 72.4 MPa | 10500 psi |
Flexural Modulus | 2.76 GPa | 400 ksi |
Izod Impact, Notched | 0.641 J/cm @Thickness 3.20 mm | 1.20 ft-lb/in @Thickness 0.126 in |
Izod Impact, Unnotched | 2.67 J/cm @Thickness 3.20 mm | 5.00 ft-lb/in @Thickness 0.126 in |
|
Electrical Properties | Metric | English | Comments |
---|
Volume Resistivity | <= 1.0 ohm-cm | <= 1.0 ohm-cm |
Surface Resistance | <= 1000 ohm | <= 1000 ohm |
Surface Resistivity per Square | <= 10000 ohm | <= 10000 ohm |
Static Decay | <= 0.50 sec | <= 0.50 sec |
Shielding Effectiveness | 52 dB @Thickness 2.00 mm, Frequency 3.00e+8 Hz | 52 dB @Thickness 0.0787 in, Frequency 3.00e+8 Hz |
| 54 dB @Thickness 2.00 mm, Frequency 5.00e+8 Hz | 54 dB @Thickness 0.0787 in, Frequency 5.00e+8 Hz |
| 58 dB @Thickness 2.00 mm, Frequency 7.00e+8 Hz | 58 dB @Thickness 0.0787 in, Frequency 7.00e+8 Hz |
| 61 dB @Thickness 2.00 mm, Frequency 1e+9 Hz | 61 dB @Thickness 0.0787 in, Frequency 1e+9 Hz |
| 64 dB @Thickness 2.00 mm, Frequency 1.30e+9 Hz | 64 dB @Thickness 0.0787 in, Frequency 1.30e+9 Hz |
| 67 dB @Thickness 2.00 mm, Frequency 1.50e+9 Hz | 67 dB @Thickness 0.0787 in, Frequency 1.50e+9 Hz |
| 68 dB @Thickness 3.00 mm, Frequency 3.00e+8 Hz | 68 dB @Thickness 0.118 in, Frequency 3.00e+8 Hz |
| 72 dB @Thickness 3.00 mm, Frequency 5.00e+8 Hz | 72 dB @Thickness 0.118 in, Frequency 5.00e+8 Hz |
| 75 dB @Thickness 3.00 mm, Frequency 7.00e+8 Hz | 75 dB @Thickness 0.118 in, Frequency 7.00e+8 Hz |
| 81 dB @Thickness 3.00 mm, Frequency 1e+9 Hz | 81 dB @Thickness 0.118 in, Frequency 1e+9 Hz |
| 84 dB @Thickness 3.00 mm, Frequency 1.30e+9 Hz | 84 dB @Thickness 0.118 in, Frequency 1.30e+9 Hz |
| 88 dB @Thickness 3.00 mm, Frequency 1.50e+9 Hz | 88 dB @Thickness 0.118 in, Frequency 1.50e+9 Hz |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear, Parallel to Flow | 61.2 µm/m-°C | 34.0 µin/in-°F |
CTE, linear, Transverse to Flow | 113 µm/m-°C | 63.0 µin/in-°F |
|
Processing Properties | Metric | English | Comments |
---|
Melt Temperature | 227 - 249 °C | 440 - 480 °F |
Mold Temperature | 65.6 - 82.2 °C | 150 - 180 °F |
Drying Temperature | 82.2 °C @Time 7200 sec | 180 °F @Time 2.00 hour |
Moisture Content | 0.10 % | 0.10 % |
Dew Point | -17.8 °C | 0.000 °F |
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.