High Impact, Extrusion & Injection Grade Typical properties; not to be construed as specifications. Mechanical properties measured on 1/8 in. Type I specimens. Information provided by US distributors Calsak Corporation and Polymer Technology and Services, LLC (PTS). |
Poly(Acrylonitrile Butadiene Styrene); Polymer Technology & Services, LLC (PTS); Calsak Corporation |