MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil Escor® AT-320 EMAAA Terpolymer for Polymer Modification  (discontinued **)
Categories: Polymer; Thermoplastic; EMAAA Terpolymer; Ethylene Methyl Acrylate

Material Notes: Data provided by the manufacturer, Exxon Chemical.

45 Acid Number. Provides unusual adhesion to a variety of substrates and other components, such as aluminum foil, polyolefins, polycarbonate, PET, etc.

Applications: Low temperature sealant; Engineering thermoplastic modifier; Heat activated sealant; Adhesive for polyolefins to metals or polar polymers.

Key Words: Ethylene Acid Terpolymer; ; Exxon Chemical Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.953 g/cc0.0344 lb/in³Exxon Method
Melt Flow 5.0 g/10 min5.0 g/10 minExxon Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8383ASTM D2240
Hardness, Shore D 3434ASTM D2240
Tensile Strength, Ultimate 76.0 MPa11000 psiASTM D638
Elongation at Break 660 %660 %ASTM D638
Tensile Impact Strength 760 kJ/m²362 ft-lb/in²23°C; ASTM D-1822
 
Thermal PropertiesMetricEnglishComments
Melting Point 76.0 °C169 °FExxon Method
Vicat Softening Point 43.0 °C109 °F1000g; ASTM D-1525
Glass Transition Temp, Tg 56.0 °C133 °FDSC

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer
ExxonMobil Escor® AT-310 EMAAA Terpolymer for Polymer Modification
Dow Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer
Dow Elvaloy® 3427 AC Ethylene and 27% Butyl Acrylate Copolymer
Dow Elvaloy® 3217 AC Ethylene and 17% Butyl Acrylate Copolymer

PEXCFA / 37922

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.