MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Spartech Royalite R632M Carbon Black Filled ABS/PVC Resin
Categories: Polymer; Thermoplastic; ABS Polymer; ABS/PVC Alloy; Vinyl (PVC)

Material Notes: Data provided by the manufacturer. This static-conductive material is UL®-listed and meets minimum static-decay requirements outlined in MIL-B-1705B and NFPA Code 56A specifications.

Key Words: Poly(Acrylonitrile-Butadiene-Styrene); Polyvinyl Chloride
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ASTM D792
Water Absorption 0.020 %0.020 %24 hrs. ASTM D570
Viscosity 212400 cP
@Shear Rate 3000 1/s,
Temperature 191 °C
212400 cP
@Shear Rate 3000 1/s,
Temperature 375 °F
Melt Viscosity
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inASTM D955
Melt Flow 0.21 g/10 min
@Load 5.00 kg,
Temperature 200 °C
0.21 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Condition G; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7272ASTM D785
Tensile Strength, Yield 31.3 MPa4540 psiASTM D638
Modulus of Elasticity 1.90 GPa276 ksiASTM D638
Flexural Yield Strength 48.4 MPa7020 psiASTM D790
Flexural Modulus 2.00 GPa290 ksiASTM D790
Izod Impact, Notched 0.900 J/cm1.69 ft-lb/inASTM D256
 0.400 J/cm
@Temperature -20.0 °C
0.749 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1e+051e+05ASTM D257
Surface Resistance 1e+051e+05ASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 166 µm/m-°C
@Temperature 20.0 °C
92.2 µin/in-°F
@Temperature 68.0 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C198 °FAnnealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C169 °FAnnealed; ASTM D648
Vicat Softening Point 80.0 °C176 °FASTM D1525
Flammability, UL94 5VA
@Thickness 2.16 mm
5VA
@Thickness 0.0850 in
Oxygen Index 30.4 %30.4 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Novatec Novaloy® 9000 PVC + ABS
Overview of materials for ABS/PVC Alloy
SEKISUI SPI KYDEX® 410 ABS/PVC
Aclo Acculoy POL063L Polycarbonate PET Alloy
Aclo Acculoy POL062L Polycarbonate PET Alloy

PROY37 / 66397

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.