See also Ceramacast™ 576-N Hydraulic setting. Medium grain castable ceramic similar to 575. Used in the production of temperature probes, electrical feed-throughs, large heat treating fixtures, induction coils and crucibles. Supplied in powder form and are mixed with water to develop a strong hydraulic bond. Typically air set in 24 hours, then cured at 250 ºF for 2-4 hours to provide maximum electrical and mechanical properties. |
casting, alumina, aluminas |
Aremco’s Ceramacast casting and potting compounds represent the most expansive line of products based on aluminum oxide, aluminum nitride, magnesium oxide, silicon dioxide, silicon carbide, zirconium oxide, and zirconium silicate for applications to 3000°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |