MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Plenco 7579 Phenolic, Granular, Injection Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Woodflour Filled

Material Notes: PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40654.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.590 g/cc0.0213 lb/in³ASTM D1895
Density 1.38 g/cc0.0499 lb/in³ASTM D792
Water Absorption 0.37 %0.37 %ASTM D570
Linear Mold Shrinkage 0.0098 cm/cm0.0098 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8282ASTM D785
Tensile Strength, Ultimate 49.0 MPa7110 psiASTM D638
Elongation at Break 0.66 %0.66 %ASTM D638
Tensile Modulus 8.30 GPa1200 ksiASTM D638
Flexural Strength 68.0 MPa9860 psiASTM D790
Flexural Modulus 6.80 GPa986 ksiASTM D790
Compressive Strength 191 MPa27700 psiASTM D695
Poissons Ratio 0.350.35ASTM D638
Shear Modulus 3.07 GPa445 ksiCalculated
Izod Impact, Notched 0.203 J/cm0.380 ft-lb/inASTM D256
Charpy Impact, Notched 0.185 J/cm²0.880 ft-lb/in²ASTM D256
Impact 140140J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.20e+11 ohm-cm3.20e+11 ohm-cmASTM D247
Dielectric Constant 5.45.4ASTM D150
Dielectric Strength 8.80 kV/mm224 kV/inShort Time; ASTM D149
Dissipation Factor 0.0630.063ASTM D150
Arc Resistance 125 sec125 secASTM D495
Comparative Tracking Index 175 V175 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 46.0 µm/m-°C
@Temperature 40.0 - 130 °C
25.6 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.380 W/m-K
@Temperature 100 °C
2.64 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 191 °C376 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 152 °C306 °FASTM D648
Flammability, UL94 V-1
@Thickness 5.10 mm
V-1
@Thickness 0.201 in
Oxygen Index 26.5 %26.5 %ASTM D2863
Shrinkage 0.46 %0.46 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 22257 Phenolic, Injection Grade

PLEM53 / 50734

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.