Ryton® R-7-190BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment. Features: Good Chemical Resistance; Good Electrical Properties; Good Strength Additional Properties: Heat Deflection Temperature - ASTM D648 265 °C; Insulation Resistance - (90°C): 1.00E+13 ohm; Mold Shrinkage - 0.20 %; Mold Shrinkage - 0.40 %; Temperature Index - UL 746B 220 to 240 °C Information provided by Solvay Specialty Polymers. |