MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Materia Proxima® HTI 1400 Polydicyclopentadiene Thermoset Resin
Categories: Polymer; Thermoset; Polydicyclopentadiene (PDCPD)

Material Notes: Materia Proxima HTI 1400 is an olefin thermoset resin designed to provide thermal insulation for temperatures up to 400°F (204°C). Proxima HTI 1400 is particularly suitable for use for subsea thermal insulation for projects in ultra-deep water applications.

Information provided by Materia, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³Polymer; ASTM D792
Water Absorption <= 0.20 %
@Temperature 100 °C
<= 0.20 %
@Temperature 212 °F
ASTM D570
Brookfield Viscosity 5.0 cP
@Temperature 30.0 °C
5.0 cP
@Temperature 86.0 °F
Resin
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7474ASTM D2240
Tensile Strength, Yield 35.0 MPa5080 psiASTM D638
Elongation at Break >= 75 %>= 75 %ASTM D638
Elongation at Yield 6.8 %6.8 %ASTM D638
Tensile Modulus 1.40 GPa203 ksiASTM D638
Compressive Strength 35.0 MPa5080 psiASTM D695
Compressive Modulus 0.001115 GPa0.1617 ksiASTM D695
Izod Impact, Notched 0.961 J/cm1.80 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.175 W/m-K1.21 BTU-in/hr-ft²-°FASTM C518
Maximum Service Temperature, Air 204 °C399 °F
Glass Transition Temp, Tg 52.0 °C126 °FDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMATERI992 / 265397

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.