MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

AGC Fluon® TL-368 Micropowder
Categories: Polymer; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP)

Material Notes: Product Description: Fluon® TL-368 is a white PTFE (polytetrafluoroethylene) micropowder, suitable for compounding in rubber and plastics. The particles of Fluon® TL-368 are of intermediate hardness, permitting mixing without further breakdown. The slight fibrous nature of Fluon® TL-368 will give greater viscosity in fluids. Fluon® TL-368 is suitable for use in food contact applications.

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.435 g/cc0.0157 lb/in³ASTM D4894
Volatiles 0.080 %0.080 %
Particle Size 12 µm12 µmHegman; ASTM D1210
 13 µm13 µmLow Shear
 40 µm40 µmLow Shear
 95 µm95 µmLow Shear
Specific Surface Area 2.5 m²/g2.5 m²/g
 
Thermal PropertiesMetricEnglishComments
Melting Point 331 °C628 °FASTM D3417
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %ASTM D4019
 
Descriptive Properties
Oil Absorption41 lb oil/100 lbASTM D1438

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAGCX286 / 191395

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.