MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Techmer ES Luriblend® PA6 CF30 TS15 BK 30% Carbon Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Carbon Fiber/PTFE Reinforced

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Carbon Fiber, 30% Filler by Weight

Additive: PTFE Lubricant (15%) and Silicone Lubricant

Features: Lubricated

Appearance: Natural Color

Processing Method: Extrusion

Information provided by TP Composites, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ASTM D792
Water Absorption 0.88 %
@Time 86400 sec
0.88 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Thickness 3.17 mm
0.0030 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 157 MPa22700 psiASTM D638
Elongation at Break 2.5 %2.5 %ASTM D638
Flexural Strength 249 MPa36100 psiASTM D790
Flexural Modulus 11.5 GPa1670 ksiASTM D790
Izod Impact, Notched 1.07 J/cm
@Thickness 3.17 mm
2.00 ft-lb/in
@Thickness 0.125 in
ASTM D256
Coefficient of Friction, Dynamic 0.100.10ASTM D1894
Coefficient of Friction, Static 0.0900.090ASTM D1894
K (wear) Factor 16.1 x 10-8 mm³/N-M8.00 x 10-10 in³-min/ft-lb-hr
Limiting Pressure Velocity 0.771 MPa-m/sec22000 psi-ft/min1000 fpm
 1.05 MPa-m/sec30000 psi-ft/min10 fpm
 1.54 MPa-m/sec44000 psi-ft/min100 fpm
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.00e+14 ohm-cm<= 1.00e+14 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C10.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 218 °C425 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 216 °C420 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Semitron® ESd 480 PEEK, static dissipative, (ASTM Product Data Sheet)
Bakelite® PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled
Cast Nylons Nycast® Nyloil® Lubricated Nylon
A. Schulman ComAlloy E-16822-1B Internally Lubricated, Carbon Fiber Reinforced Nylon 6/6

PTPC0781 / 136719

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.