Chloride and carbonate mixture recommended. For annealing nonferrous materials or for heat treating steel where slight decarburization is not desirable. Wire Annealing Salt is extremely fluid, completely water-soluble, neither hygroscopic nor corrosive, but tends to decarburize steel parts at temperatures above 1300°F. Formulated per MIL-S-10699-B, Class 3. Information provided by Heatbath Corporation - Park Metallurgical. Heatbath/Park has been acquired by DuBois Chemicals. |