MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Kolon DIAMAT® EM  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Extruded

Material Notes: Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonable pricing. DIAMAT® utilizes acrylic toughener technology resulting in consistent appearance, even after years of UV exposure. DIAMAT® EM is a resin for extrusion molding with excellent impact strength and heat resistance.

Information provided by US distributor, API-Kolon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccASTM D792
Water Absorption 0.30 %0.30 %ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inASTM D955
Melt Flow 2.6 g/10 min2.6 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7070ASTM D785
Tensile Strength, Ultimate 49.0 MPa7110 psiASTM D638
Flexural Strength 88.3 MPa12800 psiASTM D790
Flexural Modulus 2.45 GPa356 ksiASTM D790
Izod Impact, Notched 0.363 J/cm0.680 ft-lb/inASTM D256
Falling Dart Impact 10.8 J8.00 ft-lb
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C205 °FLoad not specified; ASTM D648
Vicat Softening Point 100 °C212 °FASTM D1525
Glass Transition Temp, Tg 110 °C230 °FASTM D3418
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.491.49ASTM D542
Haze <= 2.0 %<= 2.0 %ASTM D1003
Transmission, Visible 92 %92 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 150 - 180 °C302 - 356 °FInjection
Middle Barrel Temperature 180 - 230 °C356 - 446 °FInjection
Front Barrel Temperature 210 - 240 °C410 - 464 °FInjection
Nozzle Temperature 220 - 245 °C428 - 473 °FInjection
Zone 1 200 - 220 °C392 - 428 °FExtrusion
Zone 2 210 - 230 °C410 - 446 °FExtrusion
Zone 3 220 - 240 °C428 - 464 °FExtrusion
Zone 4 210 - 235 °C410 - 455 °FVent; Extrusion
Zone 5 225 - 240 °C437 - 464 °FExtrusion
Adapter Temperature 230 - 240 °C446 - 464 °FExtrusion
Die Temperature 220 - 240 °C428 - 464 °FExtrusion
Melt Temperature 220 - 235 °C428 - 455 °FRecommended for Injection
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Roll Temperature 80.0 - 100 °C176 - 212 °FExtrusion
Drying Temperature 70.0 - 80.0 °C158 - 176 °F
Dry Time 3 - 5 hour3 - 5 hour
Injection Pressure 78.45 - 137.3 MPa11380 - 19910 psi
Screw Speed 40 - 80 rpm40 - 80 rpmExtrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKOL125 / 49031

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.