MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

DuPont Mobility and Materials Hypalon® CP-337 Adhesion Primer, General Description  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Chlorosulfonated Polyethylene Rubber

Material Notes: Hypalon CP 337 is a chlorinated, medium viscosity, ethylene (meth) acrylic acid copolymer. This unique resin has been developed to improve adhesion to ethylene vinyl acetate copolymers. Hypalon CP 337 has demonstrated excellent adhesion characteristics when applied as a precoat for coatings and adhesives. It has also shown good performance when used as an additive to adhesive or coating formulations. An important feature of this resin is the acid functionality, which offers a number of formulation and processing advantages, such as:
  • Solubility in most commonly used solvents
  • Cure site for various curing mechanisms:
    • Urethane
    • Acrylic
    • Epoxy
    • Melamine
    • Azeridene

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³
Viscosity 140 cP140 cPat 20% solids (MEK/Ethyl acetate 50/50 by wt)
 
Chemical PropertiesMetricEnglishComments
Acid Value 8888Acid Number
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 14.0 °C57.2 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 1.01.0
 
Descriptive Properties
Chlorine Content35 wt%
Epoxy Resin1.5 wt%
Product FormChips

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Hypalon® 20 Chlorosulfonated Polyethylene Rubber, General Description
Dynasol Calprene® 375 Solution Random SBR
Arkema Lacovyl® GA 7701 Vinyl Copolymer

PDVJ08 / 34198

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.