MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Coosa Composites Nautical 20 38 mm Fiberglass Reinforced Polyurethane Foam Panel
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Glass Filled

Material Notes: The Nautical product is Coosa’s lightest fiberglass reinforced composite panel and an excellent replacement for plywood and other wood core composite panels due to its high strength to low weight ratio.

Nautical 20 Composite Panel: Nautical 20 is Coosa’s economical alternative in the Nautical series and the perfect middle ground between Nautical 24 and Nautical 15. With a density of 20 pounds per cubic foot, it is 45% or more lighter than plywood, providing versatility for various applications.

Information provided by Coosa Composites

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.320 g/cc0.0116 lb/in³ASTM C271
Thickness 38000 microns1500 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 3.60 MPa522 psiFlatwise; ASTM C297
Flexural Strength 15.9 MPa2310 psiASTM D790
Flexural Modulus 0.519 GPa75.3 ksiASTM D790
Compressive Strength 3.70 MPa537 psiCore; ASTM C365
Compressive Modulus 0.1337 GPa19.39 ksiCore; ASTM C365
Shear Modulus 0.0360 GPa5.22 ksiCore; ASTM C273
Shear Strength 2.90 MPa421 psiCore; ASTM C273

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOOS910 / 322930

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.