PRE-ELEC® PP 1396 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PP 1396 has excellent mechanical properties and is easy to extrude. Applications: Extrusion of conductive PP-tape. Processing: PRE-ELEC® PP 1396 compound can be extruded in the machines using normal processing conditions as with polypropylene. Test Specimen: 10[mm] wide moulded rod Information from Premix OY |