MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ExxonMobil Exceed™ 2018EB Blown Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Blow Molding Grade

Material Notes: Exceed 2018EB resin is an ethylene based polymer produced with metallocene single site catalysts using ExxonMobil Chemicals Exxpol® Technology. The higher melt index makes this polymer ideally suited for blending into LDPE rich films.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D4703 / D1505
Thickness 25.4 microns1.00 mil
Melt Flow 2.0 g/10 min2.0 g/10 minASTM D1238
Antiblock Level 2500 ppm2500 ppm
Slip Level 750 ppm750 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 480 %480 %ASTM D882
Film Elongation at Break, TD 520 %520 %ASTM D882
Coefficient of Friction 0.220.22ASTM D1894
Elmendorf Tear Strength, MD 11.0 g/micron279 g/milASTM D1922
Elmendorf Tear Strength, TD 20.0 g/micron508 g/milASTM D1922
Dart Drop 30.0 g/micron762 g/milASTM D1709
Film Tensile Strength at Break, MD 40.0 MPa5800 psiASTM D882
Film Tensile Strength at Break, TD 30.0 MPa4350 psiASTM D882
1% Secant Modulus, MD 176 MPa25500 psiASTM D882
1% Secant Modulus, TD 176 MPa25500 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 118 °C244 °FPeak Melting Temperature; ASTM D3418
 
Optical PropertiesMetricEnglishComments
Haze 6.0 %6.0 %ASTM D1003
Gloss 11 %11 %60° angle; ASTM D2457
 
Descriptive Properties
FeaturesPPA and Thermal Stabilizer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Exceed™ 4518PA Premium Cast Film Resin
ExxonMobil Exceed™ 3518 CB Premium Cast Film Resin
ExxonMobil Exceed™ 2718CB Premium Cast Film Resin
ExxonMobil Exceed™ 1015HA Metallocene Polyethylene Resin
ExxonMobil Exceed™ 1012CA Film Resin

PEXB124 / 37429

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.