MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

NOVA Chemicals Surpass® FPs016-C Octene sLLDPE Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Octene, Film

Material Notes: FPs016-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.

NOVA Chemicals' polyethylene resins are biologically and chemically inert.

Features: Outstanding melt strength, Superior toughness with excellent tear strength, Excellent seal properties, Low gel

Additives: Process stabilizer, Polymer process aid

Applications: Lamination Film, Coextruded sealant layer, High toughness film

Film properties are typical of blown film extruded on a 2.5" extruder with 4" die and 35-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.916 g/cc0.0331 lb/in³ASTM D 792
Thickness 25.0 microns0.984 milAs tested for properties on this data sheet
 12.7 - 127 microns0.500 - 5.00 milRecommended range for processing
Melt Flow 0.65 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.65 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 8.50 MPa1230 psiASTM D 882
Film Tensile Strength at Yield, TD 8.50 MPa1230 psiASTM D 882
Film Elongation at Break, MD 470 %470 %ASTM D 882
Film Elongation at Break, TD 780 %780 %ASTM D 882
Elmendorf Tear Strength MD 350 g350 gASTM D 1922
Elmendorf Tear Strength TD 430 g430 gASTM D 1922
Elmendorf Tear Strength, MD 14.0 g/micron356 g/milASTM D 1922
Elmendorf Tear Strength, TD 17.2 g/micron437 g/milASTM D 1922
Dart Drop 28.0 g/micron711 g/milASTM D 1709/A
Dart Drop Test 700 g1.54 lbF50; ASTM D 1709/A
Film Tensile Strength at Break, MD 47.0 MPa6820 psiASTM D 882
Film Tensile Strength at Break, TD 44.0 MPa6380 psiASTM D 882
1% Secant Modulus, MD 126 MPa18300 psiASTM D 882
1% Secant Modulus, TD 138 MPa20000 psiASTM D 882
Heat Seal Strength Initiation Temperature 100 °C212 °FTemperature at which a 2-mil film achieves a seal strength of 4.4N/13mm. Tested at 0.5s dwell, 0.27 N/mm² bar pressure, 305mm/min. pull speed.
 
Optical PropertiesMetricEnglishComments
Haze 7.0 %7.0 %LDPE blended; ASTM D 1003
 15 %15 %100% LLDPE; ASTM D 1003
Gloss 38 %38 %At 45°, 100% LLDPE; ASTM D 2457
 72 %72 %At 45°, LDPE blended; ASTM D 2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 185 - 220 °C365 - 428 °FRecommended
Die Opening 0.0889 - 0.216 cm0.0350 - 0.0850 inRecommended range
Blow-up Ratio (BUR) 2.0 - 3.52.0 - 3.5Optimum range
 
Descriptive Properties
Low Friction Puncture98 (J/mm)NOVA Chemicals test method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals Sclair® 11J1 Octene LLDPE Film Resin
NOVA Chemicals Surpass® FPs117-C Octene Copolymer sLLDPE Film Resins
NOVA Chemicals Surpass® FPs236-A Octene sMDPE Film Resin
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 25 Micron Film
NOVA Chemicals Surpass® FPs225-A Octene Copolymer sLLDPE Film Resin

PNOV770 / 108895

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.