MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Kumho-Sunny HW610HT AES
Categories: Polymer; Thermoplastic; AES Polymer

Material Notes: AESHW610HT is a high heat resistant AES resin, offering excellent weather resistance, high rigidity and high toughness.

Application: Park tables, skiing boards, road signals and automobile parts, etc

Features: High heat resistant; High toughness

Information provided by Shanghai Kumho Sunny Plastics co, Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D792
Maximum Moisture Content 0.0500.050
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 50.0 MPa7250 psiASTM D638
Elongation at Break 15 %15 %ASTM D638
Flexural Strength 60.0 MPa8700 psiASTM D790
Flexural Modulus 2.30 GPa334 ksiASTM D790
Izod Impact, Notched  1.40 J/cm
@Thickness 6.40 mm
2.62 ft-lb/in
@Thickness 0.252 in
5.5 J; ASTM D256
 1.80 J/cm
@Thickness 3.20 mm
3.37 ft-lb/in
@Thickness 0.126 in
5.5 J; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 103 °C217 °F120°C/hr; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C201 °F120°C/hr; ASTM D648
Vicat Softening Point 105 °C
@Load 5.00 kg
221 °F
@Load 11.0 lb
50°C/h; ASTM D1525
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 190 - 210 °C374 - 410 °F
Middle Barrel Temperature 200 - 220 °C392 - 428 °F
Front Barrel Temperature 220 - 240 °C428 - 464 °F
Nozzle Temperature 220 - 230 °C428 - 446 °F
Melt Temperature 220 - 240 °C428 - 464 °F
Mold Temperature 50.0 - 80.0 °C122 - 176 °F
Drying Temperature 80.0 - 90.0 °C176 - 194 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKMSN108 / 280960

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.