Braskem G803 LDPE Injection Molding Polyethylene
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
Low Density (LDPE)
;
Low Density Polyethylene (LDPE), Molded
Material Notes:
G803 is a low-density polyethylene with excellent processability, high fluidity, and dimensional stability. It does not contain additives. Its applications include: lids, closures, and general purpose injection molding parts.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.918
g/cc
0.0332
lb/in³
ASTM-D792
Melt Flow
30
g/10 min
@Load 2.16 kg,
Temperature 190 °C
30
g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
40
40
ASTM-D2240
Tensile Strength at Break
6.00
MPa
870
psi
ASTM-D638
Tensile Strength, Yield
9.00
MPa
1310
psi
ASTM-D638
Elongation at Break
150 %
150 %
ASTM-D638
Modulus of Rigidity
0.320
GPa
46.4
ksi
ASTM-D747
Flexural Modulus, 1% Secant
200
MPa
29000
psi
ASTM-D790
Thermal Properties
Metric
English
Comments
Vicat Softening Point
85.0
°C
@Load 1.02 kg
185
°F
@Load 2.25 lb
ASTM-D1525
Brittleness Temperature
-70.0
°C
-94.0
°F
ASTM-D746
Descriptive Properties
Temperature Profile (°C)
130-170
Injection Molding
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Braskem PB 208 LDPE Injection Molding Polyethylene
Chevron Phillips Marlex® 1009 LDPE Injection Molding Resin
LG Chemical LUTENE MB9500 LDPE Injection Molding Grade
Overview of materials for Low Density Polyethylene (LDPE), Molded
Braskem IP2418 LDPE Injection Molding Polyethylene
PBRAS906 / 106752
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.