Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-60/4 W has the following important properties:- Very high stiffness
- Good flow behavior
- Excellent oil resistance
- Easy processing
- High heat ageing resistance
Application examples are stiff injection molding parts with high resistance against heat ageing such as functional parts in the Automotive Cooling-, Heating-, and Climatic System. Part examples are charged air cooler housings and oil sump housings in the engine compartment.Information provided by EMS Grivory. |