MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler

Material Notes: Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm0.0010 - 0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0015 - 0.0025 cm/cm0.0015 - 0.0025 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  100 MPa
@Temperature 150 °C
14500 psi
@Temperature 302 °F
 120 MPa
@Temperature 120 °C
17400 psi
@Temperature 248 °F
 145 MPa
@Temperature 90.0 °C
21000 psi
@Temperature 194 °F
 160 MPa
@Temperature 60.0 °C
23200 psi
@Temperature 140 °F
 175 MPa
@Temperature 23.0 °C
25400 psi
@Temperature 73.4 °F
Elongation at Break  0.40 %
@Temperature 23.0 °C
0.40 %
@Temperature 73.4 °F
 0.50 %
@Temperature 60.0 °C
0.50 %
@Temperature 140 °F
 0.80 %
@Temperature 90.0 °C
0.80 %
@Temperature 194 °F
 1.0 %
@Temperature 120 °C
1.0 %
@Temperature 248 °F
 1.2 %
@Temperature 150 °C
1.2 %
@Temperature 302 °F
Tensile Modulus  15.0 GPa
@Temperature 150 °C
2180 ksi
@Temperature 302 °F
 22.0 GPa
@Temperature 120 °C
3190 ksi
@Temperature 248 °F
 39.0 GPa
@Temperature 90.0 °C
5660 ksi
@Temperature 194 °F
 42.0 GPa
@Temperature 60.0 °C
6090 ksi
@Temperature 140 °F
 45.0 GPa
@Temperature 23.0 °C
6530 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched 1.00 J/cm²4.76 ft-lb/in²
Charpy Impact, Notched 0.350 J/cm²1.67 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 120 ohm-cm120 ohm-cm
Surface Resistance 50 ohm50 ohm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 225 °C437 °F
Deflection Temperature at 0.46 MPa (66 psi) 280 °C536 °F
Deflection Temperature at 1.8 MPa (264 psi) 270 °C518 °F
Vicat Softening Point 255 °C
@Load 5.00 kg
491 °F
@Load 11.0 lb
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 - 310 °C554 - 590 °F
Mold Temperature 130 - 140 °C266 - 284 °F
Drying Temperature 130 - 150 °C
@Time 10800 sec
266 - 302 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced
RTP Company RTP 2291 HM  Polyetheretherketone (PEEK) Carbon Fiber 55% - High Modulus
Westlake HM 5065 High Density Polyethylene
Lotte Advanced Materials Infino® HM-4300G PPA/30% GF
Iran Petrochemical (PCC) EX 6HT HM 9455 HT High Density Polyethylene

PLATH9656 / 177352

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.