MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Prime Polymer Evolue® SP2020 LLDPE, Blown Film
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Blow Molding Grade

Material Notes: Advantages: Low Temp Heat Seal; High Speed Moldability

Major Applications: Lamination Film; Industrial Film

Information provided by Prime Polymer Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.916 g/cc0.0331 lb/in³JIS K7112
Environmental Stress Crack Resistance >= 1000 hour>= 1000 hourASTM D1693
Melt Flow 2.3 g/10 min2.3 g/10 minJIS K7210
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5454JIS K7215
Tensile Strength at Break 17.0 MPa2470 psiJIS K7161
Elongation at Break 350 %350 %Nominal; JIS K7161
Modulus of Elasticity 0.220 GPa31.9 ksiJIS K7171
Charpy Impact, Notched NBNBJIS K7111
 
Thermal PropertiesMetricEnglishComments
Melting Point 116 °C241 °FJIS K7121
Vicat Softening Point 93.0 °C199 °FJIS K7206

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRIME020 / 313413

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.