MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ascend Performance Materials Vydyne® RF00ASXS PA66-GF50
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: Vydyne RF00ASXS is a 50% glass fiber reinforced PA66 for injection molded applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³DAM; ISO 1183
Water Absorption 0.70 %
@Time 86400 sec
0.70 %
@Time 24.0 hour
DAM; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 210 MPa30500 psiDAM; ISO 527-2
Elongation at Break 2.4 %2.4 %DAM; ISO 527-2
Tensile Modulus 15.4 GPa2230 ksiDAM; ISO 527-2
Flexural Strength 305 MPa44200 psiDAM; ISO 178
Flexural Modulus 14.1 GPa2050 ksiDAM; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 259 °C498 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 246 °C475 °FUnannealed; DAM; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 - 280 °C500 - 536 °FInjection
Middle Barrel Temperature 270 - 280 °C518 - 536 °FInjection
Front Barrel Temperature 270 - 280 °C518 - 536 °FInjection
Nozzle Temperature 270 - 280 °C518 - 536 °FInjection
Melt Temperature 270 - 280 °C518 - 536 °FInjection
Mold Temperature 60.0 - 90.0 °C140 - 194 °FInjection
Drying Temperature 70.0 - 90.0 °C158 - 194 °FInjection
Dry Time 4.00 hour4.00 hourInjection
Moisture Content 0.20 %0.20 %Injection
 
Descriptive Properties
AdditiveRelease agent
Agency RatingsISO, 1043 PA66 GF50
AppearanceNatural Color
FeaturesHigh Rigidity
 High Strength
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE8545 / 296322

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.