MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Syensqo (Solvay Specialty Polymers) Ryton® R-4-222NA Polyphenylene Sulfide (PPS), 40% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: Ryton® R-4-222NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water and complies with United States Food and Drug Administration (FDA) and European Union (EU 10/2011 and 1183/2012) regulations for use as a component of articles intended for repeat use in contact with all types of foods.

Features: Food Contact Acceptable; Good Strength

Additional Properties: Hydrolytic Stability - > 80 %; Hydrolytic Stability - < 1.0 %

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0607 lb/in³ASTM D792
Filler Content 40 %40 %Glass Fiber
Water Absorption 0.020 %
@Time 86400 sec
0.020 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Thickness 3.18 mm
0.0020 in/in
@Thickness 0.125 in
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
@Thickness 3.20 mm
0.0050 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 103103ASTM D785
Hardness, Rockwell R 122122ASTM D785
Tensile Strength 186 MPa27000 psiASTM D638
Tensile Stress 190 MPa27600 psiISO 527-2
Elongation at Break 1.6 %1.6 %ISO 527-2
 1.6 %1.6 %ASTM D638
Flexural Strength 269 MPa39000 psiASTM D790
 275 MPa39900 psiISO 178
Flexural Modulus 14.0 GPa2030 ksiISO 178
 14.5 GPa2100 ksiASTM D790
Compressive Strength 275 MPa39900 psiASTM D695
Poissons Ratio 0.370.37ASTM E132
Izod Impact, Notched 0.910 J/cm
@Thickness 3.18 mm
1.70 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 6.40 J/cm
@Thickness 3.18 mm
12.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Notched (ISO) 9.00 kJ/m²4.28 ft-lb/in²Notch A; ISO 180
Izod Impact, Unnotched (ISO) 35.0 kJ/m²16.7 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohm1.00e+16 ohmASTM D257
Dielectric Constant  3.8
@Frequency 1000 Hz
3.8
@Frequency 1000 Hz
ASTM D150
 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 22.0 kV/mm559 kV/inASTM D149
Dissipation Factor  0.0020
@Frequency 1000 Hz
0.0020
@Frequency 1000 Hz
ASTM D150
 0.0030
@Frequency 1e+6 Hz
0.0030
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 125 sec125 secASTM D495
Comparative Tracking Index 150 V150 VUL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  15.0 µm/m-°C
@Temperature 100 - 200 °C
8.33 µin/in-°F
@Temperature 212 - 392 °F
 15.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F
@Temperature -58.0 - 122 °F
CTE, linear, Transverse to Flow  40.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
22.2 µin/in-°F
@Temperature -58.0 - 122 °F
TMA; ASTM E831
 85.0 µm/m-°C
@Temperature 100 - 200 °C
47.2 µin/in-°F
@Temperature 212 - 392 °F
TMA; ASTM E831
Thermal Conductivity 0.310 W/m-K2.15 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 265 °C509 °FUnannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Oxygen Index 45 %45 %ASTM D2863
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Agency RatingsEU 10/2011; FDA Food Contact
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorNatural
FormPellets
Processing TechniqueInjection Molding
RoHS ComplianceRoHS Compliant

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

PSOL8Y7265 / 176996

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.