MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger XP-132 Compression Molded PI Compound, 15% Graphite Filled
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Graphite Filled

Material Notes: The XP-130 is an amorphous high performance thermoplastic with high permanent temperature and creep resistance as well as excellent bearing and wear properties, excellent long term thermal stability and creep resistance.

The XP 130 Series of Polyimide is a non-melting high temperature thermoplastic with high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance along with good chemical resistance.

Applications:

  • Thermal & electrical insulators
  • Switch Parts
  • Vacuum Seals
  • Plug Parts
  • Chip Carriers
  • Hot glass gripper fingers
  • Balls for control valves
  • Housing Parts
  • Welding Equipment

Information provided by Ensinger Special Polymers, Inc.

Vendors: Ensinger Special Polymers, Inc. provides consistent, high quality compression molded stock shapes of engineering thermoplastics. Common shapes include rings, rods, plates, tubes, and discs. Large diameter rings up to 90" OD are available.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ASTM D792
Filler Content 15 %15 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 119119ASTM D785
Tensile Strength 96.5 MPa14000 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Strength 101 MPa14700 psiASTM D790
 
Descriptive Properties
ColorDark Brown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger XP-151 Compression Molded PI Compound, 15% Graphite Filled, Premium Grade
Ensinger TECASINT 3062 Polyimide, Shiny Black, 15% Graphite, 10% PTFE (PI)
Ensinger TECASINT 4041 Polyimide, Glossy Black, Molybdenum Sulfide (PI)
Ensinger TECASINT 4201 SD Polyimide, Black, Carbon Fiber (PI)
Ensinger TECASINT 4211 SD Polyimide, Black, Carbon Fiber (PI)

PENSIN967 / 140840

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.