MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ExxonMobil Optema™ TC 221 ExCo Ethylene Methyl Acrylate, Extrusion Coating Grade
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Coating Grade

Material Notes: Optema™ TC 221 is an ethylene methyl acrylate copolymer that can be used for making alloys, blends and compounds. It can also be injection molded where softness and flexibility are required. It is an excellent grade for coextrusion coating and extrusion lamination where good interlayer adhesion between poylethylene, polypropylene, nylon, PVdC, or other substrates is required

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ASTM D1505
Methyl Acrylate Content 24 %24 %ExxonMobil Method
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Neck In  10.7 cm
@Temperature 295 °C
4.20 in
@Temperature 563 °F
656 ft/min, constant output @ 35 rpm; ExxonMobil Method
 14.0 cm
@Temperature 295 °C
5.50 in
@Temperature 563 °F
328 ft/min, constant output @ 35 rpm; ExxonMobil Method
 
Thermal PropertiesMetricEnglishComments
Melting Point 73.3 °C164 °FPeak; ExxonMobil Method
Vicat Softening Point 45.6 °C114 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEX98902 / 238284

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.