MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Poly Alloy Etoma™ ET6211 ABS with carbon black
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Conductive

Material Notes: Etoma ET6211 resin is a conductive compound based on acrylonitrile butadiene styrene (ABS) with carbon black. The carbon black makes electrical conductive on material permanently . With special formula, ET6211 has perfect mechanical properties and is easy to extrude and injection mold. Typical applications include IC trays, holder, mechanical parts.

Information provided by Poly Alloy Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.105 g/cc1.105 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 42.2 MPa6120 psiASTM D638
Elongation at Break 4.0 %4.0 %ASTM D638
Flexural Strength 59.8 MPa8680 psiASTM D790
Flexural Modulus 2.94 GPa427 ksiASTM D790
Izod Impact, Notched 0.294 J/cm0.551 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1000 ohm - 1e+051000 ohm - 1e+05ASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 1 200 - 210 °C392 - 410 °F
Zone 2 210 - 230 °C410 - 446 °F
Zone 3 210 - 230 °C410 - 446 °F
Zone 4 210 - 230 °C410 - 446 °F
Die Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 hour2.00 hour
Shelf Life 24.0 Month24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPALLOY050 / 278329

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.