MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lubrizol Advanced Materials Carbo-Rite™ M-2530 High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with Carbon Black Filler

Material Notes: Product Description: M-2530 is a carbon black-filled HIPS compound available in pellet form. It solves a wide range of static decay, static shielding and electromagnetic shielding problems. Applications: Thermoformed trays, Tape & Reel Carrier Tape, Extruded conductive HIPS sheet.
Availability: Asia Pacific, Europe, Latin America, North America
Filler/Reinforcement: Carbon Black
Features: Consistent Performance; Durable; Electromagnetic Shielding (EMI); Cost-effective ESD protection; Recyclable Material
Uses: Electrical/Electronic Applications; Sheet; Tape
Appearance: Black
Forms: Pellets
Processing Method: Sheet Extrusion; Thermoforming

Information provided by Lubrizol Advanced Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ASTM D792
Water Absorption 0.010 %
@Time 86400 sec
0.010 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm0.010 - 0.012 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 24.0 MPa3480 psiASTM D638
Elongation at Break 16 %16 %ASTM D638
Tensile Modulus 1.36 GPa197 ksiASTM D638
Flexural Modulus 2.07 GPa300 ksiASTM D790
Izod Impact, Notched 1.87 J/cm3.50 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 5.00e+6 ohm-cm<= 5.00e+6 ohm-cm12% RH; ESD S11.12
Surface Resistance <= 50000 ohm<= 50000 ohm12% RH; ESD S11.11
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 62.2 °C144 °FUnannealed; ASTM D648
 
Descriptive Properties
Ionic Content<0.01 ng/cm2Anions Cl
Outgassing0.0 µg/cm2MMA
 12 µg/cm2Toluene
 290 µg/cm2Styrene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUBR6008 / 268310

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.