MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

AISI Type O7 Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel; Cold Work Steel; Oil-Hardening Steel

Material Notes: General purpose, oil-hardening, nondeforming alloy tool steel suitable for applications where extreme dimensional accuracy is required. Applications include punches, dies, and knives where a keen cutting edge is required.

Key Words: AISI Oil-Hardening Tool Steel O7, UNS T31507, ASTM A681, FED QQ-T-570, oil-hardening, non-deforming alloy tool steel suitable, dimensional accuracy, wear resistant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 58 - 6458 - 64
Bulk Modulus 160 GPa23200 ksiTypical for steels.
Machinability 85 %85 %Based on 1% carbon water-hardening tool steel.
Shear Modulus 80.0 GPa11600 ksiTypical for steels.
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.2 µm/m-°C6.22 µin/in-°F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 290 °C347 - 554 °FTempering Temperature
 790 - 885 °C1450 - 1630 °FHardening Temperature
Annealing Temperature 790 - 815 °C1450 - 1500 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.1 - 1.3 %1.1 - 1.3 %
Chromium, Cr 0.60 %0.60 %
Iron, Fe 94 %94 %As Balance
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo <= 0.30 %<= 0.30 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si <= 0.60 %<= 0.60 %
Sulfur, S <= 0.030 %<= 0.030 %
Tungsten, W 1.5 %1.5 %
Vanadium, V <= 0.40 %<= 0.40 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type O6 Tool Steel
AISI Type O2 Oil-hardening Tool Steel, oil quenched at 800°C, tempered at 260°C
AISI Type A2 Tool Steel
AISI Type A6 Tool Steel
AISI Type A7 Tool Steel

MSTO7A / 14105

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.