MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Plenco 7552 Phenolic, Nodular, Injection Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Glass Filled

Material Notes: PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL recognized under component file E40654.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.670 g/cc0.0242 lb/in³ASTM D1895
Density 1.72 g/cc0.0621 lb/in³ASTM D792
Water Absorption 0.121 %0.121 %ASTM D570
Linear Mold Shrinkage 0.0049 cm/cm0.0049 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8181ASTM D785
Tensile Strength, Ultimate 43.0 MPa6240 psiASTM D638
Elongation at Break 0.51 %0.51 %ASTM D638
Tensile Modulus 11.7 GPa1700 ksiASTM D638
Flexural Strength 75.0 MPa10900 psiASTM D790
Flexural Modulus 10.3 GPa1490 ksiASTM D790
Compressive Strength 156 MPa22600 psiASTM D695
Poissons Ratio 0.310.31ASTM D638
Shear Modulus 4.47 GPa648 ksiCalculated
Izod Impact, Notched 0.340 J/cm0.637 ft-lb/inASTM D256
Charpy Impact, Notched 0.310 J/cm²1.48 ft-lb/in²ASTM D256
Impact 188188J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.60e+12 ohm-cm2.60e+12 ohm-cmASTM D247
Dielectric Constant 4.94.9ASTM D150
Dielectric Strength 13.6 kV/mm345 kV/inShort Time; ASTM D149
Dissipation Factor 0.0390.039ASTM D150
Arc Resistance 184 sec184 secASTM D495
Comparative Tracking Index 200 V200 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 35.0 µm/m-°C
@Temperature 40.0 - 130 °C
19.4 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.580 W/m-K
@Temperature 100 °C
4.03 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 189 °C372 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 261 °C502 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Oxygen Index 46 %46 %ASTM D2863
Shrinkage 0.103 %0.103 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLEM48 / 50729

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.