MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

INEOS Styrolution Terblend® N NG-04EF SL ABS+PA, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced

Material Notes: Product Description: Terblend® N NG-04EF SL is a 20% glass fiber reinforced UV-stabilized ABS/PA blend with enhanced dimensional stability, rigidity and high flowability that was developed to give the best performance as back injection molding material for StyLight thermoplastic composites.
Features: High dimensional stability; Low shrinkage; Enhanced softening temperature; Enhanced rigidity; Glass Fiber reinforced (30%)
Applications: Back injection molding material for StyLight

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Filler/Reinforcement: Glass Fiber, 20% Filler by Weight

Additive: UV Stabilizer

Features: Good Rigidity; High Dimensional Stability; High Flow; Low Shrinkage; UV Stabilized

Form: Pellets

Processing Method: Injection Molding

Information provided by INEOS Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ISO 1183
Water Absorption at Saturation 4.4 %4.4 %ASTM D570
Melt Flow  30 g/10 min
@Load 10.0 kg,
Temperature 220 °C
30 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 30 g/10 min
@Load 10.0 kg,
Temperature 240 °C
30 g/10 min
@Load 22.0 lb,
Temperature 464 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 77.9 MPa11300 psiISO 527-2
Elongation at Yield 4.0 %4.0 %ISO 527-2
Flexural Strength 109 MPa15800 psiISO 178
Flexural Modulus 4.18 GPa606 ksiISO 178
Charpy Impact Unnotched  5.04 J/cm²
@Temperature -30.0 °C
24.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 5.25 J/cm²
@Temperature 22.8 °C
25.0 ft-lb/in²
@Temperature 73.0 °F
ISO 179
Charpy Impact, Notched  0.798 J/cm²
@Temperature -30.0 °C
3.80 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.20 J/cm²
@Temperature 22.8 °C
5.70 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 190 °C374 °FAnnealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 108 °C226 °FAnnealed; ISO 75-2/A
Vicat Softening Point 125 °C257 °FISO 306/B50
 195 °C383 °FISO 306/A50
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 270 °C464 - 518 °F
Mold Temperature 80.0 °C176 °F
Dry Time 4.00 hour4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSTYS776 / 311469

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.