  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

BIW ASTM Class 2D0 Silicone Foam
Categories: Polymer; Thermoset; Silicone; Silicone Foam

Material Notes: Products are a closed cell foam and therefor good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters.

Information provided by BIW Isolierstoffe GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density <= 0.280 g/cc<= 0.0101 lb/in³DIN 53479 A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A <= 5<= 5DIN 53505
Compressive Yield Strength <= 0.0150 MPa<= 2.18 psi25% Compression
Compression Set <= 80 %
@Temperature 100 °C,
Time 79200 sec
<= 80 %
@Temperature 212 °F,
Time 22.0 hour
50% Compression
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 °C356 °FStandard Quality, All Colors
 280 °C536 °FHighly Temperature Resistant Quality, Opaque, Grey, Blue
Minimum Service Temperature, Air -60.0 °C-76.0 °FStandard Quality, All Colors

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Foam
Multibase Multi-Flex® A 2504LC TPE Thermoplastic Elastomer
Rogers Corporation R/bak® SS Cushion Mounting Materials, Supported Soft
Rogers Corporation Poron® 4701-30-25 Urethane Foam, Very Soft
General Plastics LAST-A-FOAM® FR-3803 FST Polyurethane Foam

PBIWS990 / 155886

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.