MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Saint-Gobain COHRlastic® R10460 Medium Flame Retardant Silicone Sponge Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Foam

Material Notes: Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six constructions. R10460 is flame retardant. When held in a vertical position and exposed to a 2,000°F flame for 12 seconds, there is no residential flame and less than a 10 second afterglow. Like R10480, it is especially resistant to compression set.
Specification Notes: Meets Specifications: AMS 3195, MIL-R-6130 Type II, Grade B&C, MIL-R-46089, Boeing BMS 1-23, Boeing BMS 1-60 Type I, Grade B, Douglas DMS 1597, Douglas DMS 1980, Grade 2, MIL-R-6130 Type II, Grade A. All data based on a 0.0625 inch test sample.(Other thicknesses available.)
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.471 g/cc0.0170 lb/in³ASTM D3574
Water Absorption <= 5.0 %<= 5.0 %ASTM D1056
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 0.517 MPa75.0 psiASTM D412
Elongation at Break 125 %125 %ASTM D412
Compressive Strength 0.0689 MPa
@Temperature 23.0 °C
10.0 psi
@Temperature 73.4 °F
ASTM D1056
Compression Set 5.0 %5.0 %ASTM D1056
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 5.71 kV/mm145 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 324 µm/m-°C
@Temperature 20.0 - 177 °C
180 µin/in-°F
@Temperature 68.0 - 350 °F
Specific Heat Capacity 1.26 J/g-°C0.300 BTU/lb-°F
Thermal Conductivity 0.108 W/m-K0.750 BTU-in/hr-ft²-°F
 
Descriptive Properties
ColorDark Blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSTGQZ256 / 68770

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.